Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADILON ADLINE CS - PA666 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADILON ADLINE CS:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radilon A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
PA6/66 copolymer for 3D Printing Fused Deposition Modelling.

Suitable for parts requiring high dimensional stability and very reduced shrinkage. Transparent material, it offers good surface aspect and easy processability.
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2005 / - MPa ISO 527
Tensão no escoamento 55 / - MPa ISO 527
Deformação no escoamento 4.5 / - % ISO 527
Deformação nominal na ruptura 15 / - % ISO 527
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 30 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 195 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 45 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 50 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 10.2 / * % Sim. to ISO 62
Absorção de umidade 3 / * % Sim. to ISO 62
Densidade 1100 / - kg/m³ ISO 1183
Características
Processamento
Additive Manufacturing
Forma de entrega
Granulado
Características especiais
Transparente
Características
Copolímero
Disponibilidade regional
Outras informações
Moldagem por injeção
The material is available in granules or in filament – 1.75 mm and 2.85 mm diameter.
In the case of granules, the material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.10%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. In the case of filaments, the material is originally sealed in vacuum bags with silica gel inside to keep environment in dry conditions. For best printing results, it is recommended to pre-dry the filament at 70-80°C for 2-4 h or more. Alternatively, Radilon® Adline filaments are compatible with Drywise system from Thought3D Ltd. 

Recommended 3D-Print processing parameters:
 
Nozzle Temperature Bed Temperature Adhesion promoter Print Speed
250°-280°C 70-100°C Magigoo glue 30-40 mm/s


Please note: Parameters are dependent on printer used.
Radici tests were performed on a Ultimaker S5 printer
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.